Many years ago I sent out a convertible windshield which was pot medal-die cast, that the chrome player left in the stripping tank way too long. It came out looking like Swiss cheese. It initially looked like scrap metal but I had an old friend who was a skill aircraft welder who was a master craftsman. Over many hours and days he was able to save the windshield. He had to heat the windshield in an over to a high temperature but below melting the windshield and take in out and braze new metal into the windshield. It was a very slow process into the oven and out again to weld. He then gave me back the windshield and I then had to hand file all the repaired areas. I then gave it back to the chrome platter and he only copper plated it. He gave it back to me and I hand wet sanded the windshield to remove the last of the imperfections. I then gave it back to the chrome plater to finish the chrome platting.
You donÔÇÖt have as much a headache chrome platting the brass windshield but the pot metal Cord windshields do fit the car better.
About 15 years ago I had some bronze phaeoton windshield frames cast because my original pot metal ones were pitted badly.  To keep costs down for the patternmaking and casting I did not have the window glass groove put in.  I felt it was better to cut it in after the frames were fitted to my car.  I never did get around to getting them machined.  I chromed my original ones and I recently noticed the chrome is bubbled in places and they are not even on the car yet.  I could end up getting a set machined for my car.  I do have a couple of extra sets left.  They will have to be machined and polished.  There was extra material added to the patterns to allow for shrinkage and differences between each car.
Tom
I have a pot metal left side in fair condition. detail missing on corners and thin at top
mmsfld@aol.com
To join in the conversation, you must be a club member.
You’re welcome to read and like every post. Members can reply and start topics of their own.